Polyamide 6 (PA6)
PA6-GF10 Taromid B 280 G2
Manufacturer:Not recorded
Recorded properties
Record date:2026-11-07
| Property | Value | Unit |
|---|---|---|
| Density | 1.18 | g/cm³ |
| Melt flow rate | 2.16 | g/10min |
| Tensile strength | 105.0 | MPa |
| Tensile modulus | 4700.0 | MPa |
| Elongation at break | 7.0 | % |
| Flexural modulus | 4500.0 | MPa |
| Notched impact strength | 5.0 | kJ/m² |
| HDT 1.8MPa | 90.0 | °C |
| Vicat softening point | 214.0 | °C |
| Flame rating | HB - UL 94 | — |
Test standard, specimen condition and source rights are not fully recorded. Values are for preliminary screening only; verify with the manufacturer before design or purchasing decisions.