PA6+PP-GF20
PA6+PP-GF20_AKROMID® B3 GF 20 9 L natural
Manufacturer:阿克罗塑料公司
注塑成型
Recorded properties
Record date:2026-11-07
| Property | Value | Unit |
|---|---|---|
| Melt flow rate | 19.0 | g/10min |
| Tensile strength | 117.0 | MPa |
| Tensile modulus | 6300.0 | MPa |
| Elongation at break | 4.2 | % |
| Notched impact strength | 16.0 | kJ/m² |
Test standard, specimen condition and source rights are not fully recorded. Values are for preliminary screening only; verify with the manufacturer before design or purchasing decisions.
Grade handling information to verify
The information below was automatically extracted from a material PDF and has not been individually reviewed. It is for preliminary reference only. Verify the exact grade’s manufacturer processing instructions, safety data sheet and equipment procedures before production; do not use candidate values directly as machine settings.
Matched by original PDF filename
- Storage
- Review the source for packaging, storage and opened-package instructions.
- Drying
- No drying value was confirmed by extraction; review the source.
- Equipment setup
- Candidate injection-molding recommendations: melt temperature 270 °C; mold temperature 80 °C. Verify the source, grade and conditions.
- Applications
- Candidate application areas in the source: automotive, electrical and electronics. Verify the source, exact use and applicable approvals.
Source: the matched material PDF; page numbers refer to the original PDF.
- Melt temperature:page 1
- Mold temperature:page 1
- Application areas:page 1