Polyester Elastomer

LUBRICOMP™ Compound YL003C

Manufacturer:LNP™

LNP清洁混合技术,耐磨

Recorded properties

Record date:2026-11-08

PropertyValueUnit
Density1.27g/cm³
Tensile strength22.0MPa
Tensile modulus260.0MPa
Elongation at break50.0%
Flexural strength12.0MPa
Flexural modulus280.0MPa
Notched impact strength23.0kJ/m²
HDT 1.8MPa57.0°C
HDT 0.45MPa88.0°C

Test standard, specimen condition and source rights are not fully recorded. Values are for preliminary screening only; verify with the manufacturer before design or purchasing decisions.

Grade handling information to verify

The information below was automatically extracted from a material PDF and has not been individually reviewed. It is for preliminary reference only. Verify the exact grade’s manufacturer processing instructions, safety data sheet and equipment procedures before production; do not use candidate values directly as machine settings.

Matched by original PDF filename

Storage
Review the source for packaging, storage and opened-package instructions.
Drying
Candidate injection-molding recommendations: temperature 80 °C; time 4 h; processing moisture ≤0.1 %. Verify the source, grade and conditions.
Equipment setup
Candidate injection-molding recommendations: melt temperature 215 - 240 °C; mold temperature 25 - 55 °C. Verify the source, grade and conditions.
Applications
Review the source and applicable approvals.

Source: the matched material PDF; page numbers refer to the original PDF.

  • Drying temperature:page 1
  • Drying time:page 1
  • Processing moisture:page 1
  • Melt temperature:page 1
  • Mold temperature:page 1