thermoplastic polyester elastomer
672
Manufacturer:瑞泰弗莱克斯
高模量
Recorded properties
Record date:2026-11-08
| Property | Value | Unit |
|---|---|---|
| Density | 1.26 | g/cm³ |
| Tensile strength | 25.0 | MPa |
| Tensile modulus | 475.0 | MPa |
| Elongation at break | 50.0 | % |
| Notched impact strength | 19.0 | kJ/m² |
| HDT 1.8MPa | 100.0 | °C |
| HDT 0.45MPa | 100.0 | °C |
Test standard, specimen condition and source rights are not fully recorded. Values are for preliminary screening only; verify with the manufacturer before design or purchasing decisions.
Grade handling information to verify
The information below was automatically extracted from a material PDF and has not been individually reviewed. It is for preliminary reference only. Verify the exact grade’s manufacturer processing instructions, safety data sheet and equipment procedures before production; do not use candidate values directly as machine settings.
Matched by original PDF filename
- Storage
- Review the source for packaging, storage and opened-package instructions.
- Drying
- Candidate injection-molding recommendations: temperature 121 °C; time 4 h; processing moisture ≤0.05 %. Verify the source, grade and conditions.
- Equipment setup
- Candidate injection-molding recommendations: melt temperature 220 - 235 °C; mold temperature 20 - 55 °C. Verify the source, grade and conditions.
- Applications
- Review the source and applicable approvals.
Source: the matched material PDF; page numbers refer to the original PDF.
- Drying temperature:page 1
- Drying time:page 1
- Processing moisture:page 1
- Melt temperature:page 1
- Mold temperature:page 1