PP

PP-T40

Manufacturer:Not recorded

Recorded properties

Record date:2026-11-08

PropertyValueUnit
Density1.3g/cm³
Melt flow rate6.0g/10min
Tensile strength29.6MPa
Tensile modulus5170.0MPa
Elongation at break15.0%
Flexural strength60.7MPa
Flexural modulus4210.0MPa
Notched impact strength27.0kJ/m²
HDT 1.8MPa143.0°C
HDT 0.45MPa104.0°C

Test standard, specimen condition and source rights are not fully recorded. Values are for preliminary screening only; verify with the manufacturer before design or purchasing decisions.

Grade handling information to verify

The information below was automatically extracted from a material PDF and has not been individually reviewed. It is for preliminary reference only. Verify the exact grade’s manufacturer processing instructions, safety data sheet and equipment procedures before production; do not use candidate values directly as machine settings.

Matched by original PDF filename

Storage
Review the source for packaging, storage and opened-package instructions.
Drying
Candidate injection-molding recommendations: temperature 77 °C; time 2 h; processing moisture ≤0.2 %. Verify the source, grade and conditions.
Equipment setup
Candidate injection-molding recommendations: melt temperature 199 - 232 °C; mold temperature 32 - 71 °C. Verify the source, grade and conditions.
Applications
Review the source and applicable approvals.

Source: the matched material PDF; page numbers refer to the original PDF.

  • Drying temperature:page 1
  • Drying time:page 1
  • Processing moisture:page 1
  • Melt temperature:page 1
  • Mold temperature:page 1