PP (Polypropylene)

PP-T10_Haiplen EP50 T2 X2

Manufacturer:Not recorded

Recorded properties

Record date:2026-11-08

PropertyValueUnit
Density1.03g/cm³
Melt flow rate14.0g/10min
Tensile strength30.0MPa
Elongation at break30.0%
Flexural modulus1700.0MPa
HDT 1.8MPa65.0°C
HDT 0.45MPa100.0°C
Vicat softening point152.0°C
Flame ratingV-2—

Test standard, specimen condition and source rights are not fully recorded. Values are for preliminary screening only; verify with the manufacturer before design or purchasing decisions.

Grade handling information to verify

The information below was automatically extracted from a material PDF and has not been individually reviewed. It is for preliminary reference only. Verify the exact grade’s manufacturer processing instructions, safety data sheet and equipment procedures before production; do not use candidate values directly as machine settings.

Matched by original PDF filename

Storage
Review the source for packaging, storage and opened-package instructions.
Drying
No drying value was confirmed by extraction; review the source.
Equipment setup
No equipment setting was confirmed by extraction; review the source.
Applications
Candidate application areas in the source: automotive, electrical and electronics. Verify the source, exact use and applicable approvals.

Source: the matched material PDF; page numbers refer to the original PDF.

  • Application areas:page 1