PP (Polypropylene)

PP-K42_INNOPOL® CS 1-1240 I-160

Manufacturer:Not recorded

Recorded properties

Record date:2026-11-08

PropertyValueUnit
Density1.24g/cm³
Melt flow rate22.0g/10min
Tensile strength25.0MPa
Tensile modulus2900.0MPa
Elongation at break3.0%
Flexural modulus3250.0MPa
Notched impact strength3.7kJ/m²
HDT 1.8MPa119.0°C

Test standard, specimen condition and source rights are not fully recorded. Values are for preliminary screening only; verify with the manufacturer before design or purchasing decisions.

Grade handling information to verify

The information below was automatically extracted from a material PDF and has not been individually reviewed. It is for preliminary reference only. Verify the exact grade’s manufacturer processing instructions, safety data sheet and equipment procedures before production; do not use candidate values directly as machine settings.

Matched by original PDF filename

Storage
Review the source for packaging, storage and opened-package instructions.
Drying
Candidate injection-molding recommendations: temperature 80 °C; time 2 h; processing moisture ≤0.07 %. Verify the source, grade and conditions.
Equipment setup
Candidate injection-molding recommendations: melt temperature 230 - 260 °C; mold temperature 10 - 50 °C. Verify the source, grade and conditions.
Applications
Review the source and applicable approvals.

Source: the matched material PDF; page numbers refer to the original PDF.

  • Drying temperature:page 1
  • Drying time:page 1
  • Processing moisture:page 1
  • Melt temperature:page 1
  • Mold temperature:page 1